All-ceramic biomaterials
(Part one)
2017
 All-ceramics contain a large amount of crystalline
phase (35–99 vol%), which is responsible for
improving mechanical properties.
Types of all-ceramic materials
1. Sintered all-ceramic materials
2. Castable glass ceramics
3. Heat-pressed ceramics
4. Glass-infiltrated ceramics (slip-cast ceramics)
5. Machined ceramics
Types Subtypes Crystals percentage
1. Sintered
(not available)
Alumina-based Alumina 40–50 wt%
Leucite-reinforced Leucite 45 vol%
2. Castable
(not available)
Mica 45%
3. Heat-
pressed
Leucite-reinforced Leucite 35–45 vol%
Lithium disilicate Lithium disilicate 65 vol%
4. Glass-
infiltrated
(slip-cast)
In-Ceram Alumina Alumina 68 vol%
In-Ceram Spinel Magnesia & alumina
In-Ceram Zirconia Alumina
12Ce-TZP
34 vol%
33 vol%
12Ce-TZP: zirconia stabilized with 12 mol% ceria .
All-ceramic materials
Translucency
Leucite > Lithium disilicate & Magnesia > Alumina > Zirconia-based ceramics.
Flexural strength
Leucite < Lithium disilicate & Magnesia < Alumina < Zirconia-based ceramics.
(150) (300) (350–400) (550–600) (650–1400 Mpa)
Highest fracture toughness: zirconia-based ceramics (3Y-TZP & Ce-TZP/A).
 3Y-TZP: Yttria partially stabilized tetragonal zirconia polycrystals.
 Ce-TZP/A: ceria stabilized zirconia/alumina nanocomposite .
Highest elastic modulus: alumina-based ceramics (Procera).
1. Sintered all-ceramic materials
Types
1.1. Alumina-based ceramics
1.2. Leucite-reinforced ceramics
Porcelain furnace
1.1. Alumina-based ceramics
 By McLean in 1965.
 Alumina crystals: 40–50% by weight.
 Flexural strength: about 140 MPa (about
twice that of feldspathic porcelain).
1.1. Alumina-based ceramics
(continued)
 Higher elastic modulus and fracture toughness
compared to feldspathic porcelain.
 Veneered with matched-expansion porcelain.
1.2. Leucite-reinforced ceramics
* Leucite crystals: up to 45 vol%.
* Flexural strength: 104 MPa.
* High thermal contraction coefficient.
1.2. Leucite-reinforced ceramics
(continued)
 Large mismatch in thermal contraction between
leucite crystals and glass matrix results in
tangential compressive stresses in the glass
around leucite crystals.
 These stresses act as crack deflectors and
increase the resistance to crack propagation.
Note: Sintered all-ceramic restorations are now
being replaced by heat pressed or machined all-
ceramic restorations.
2. Castable glass ceramics
 In 1980s.
 Example: Dicor (Dentsply).
 Tetrasilicic fluormica crystals: 45%
& glass matrix.
2. Castable glass ceramics
(continued)
 Made using the lost-wax technique.
 Flexural strength: about 150 MPa.
 No longer available in the market.
3. Heat-pressed ceramics
 In the early 1990s.
 Pressed at high temperature (920–1180°C)
for 20 min in a phosphate-bonded investment
mold produced by the lost-wax technique.
 Advantages: * Short processing times.
* Good esthetics.
3. Heat-pressed ceramics
(continued)
Disadvantages
 Relatively lower strength compared to alumina
and zirconia slip-cast and machinable.
 Relatively inexpensive equipments.
Types: 3.1. Leucite-reinforced glass ceramics.
3.2. Lithium disilicate glass-ceramics.
Lost-wax and heat-pressing techniques
Heat-pressing furnace
3.1. Leucite-reinforced glass ceramics
 First generation.
 Example: IPS Empress (Ivoclar Vivadent).
 Leucite crystals: 35–45 vol%
dispersed in a glassy matrix.
 Porosity: about 9%.
 The molding procedure is conducted at 1080°C
for about 20 min.
(A) Feldspathic dental porcelain. (B) Leucite-reinforced ceramic.
3.1. Leucite-reinforced glass ceramics
(continued)
 Tangential compressive stresses develop
around the crystals on cooling because of the
difference in the coefficient of thermal expansion
(CTE) between leucite crystals and the glassy
matrix.
 These stresses contribute to crack deflection
and improved mechanical performance.
3.1. Leucite-reinforced glass ceramics
(continued)
 Flexural strength and fracture toughness values
are about double those of feldspathic porcelains.
 Flexural strength: about 150 MPa.
 Indications: inlays, onlays, veneers and anterior
crowns.
3.1. Leucite-reinforced glass ceramics
(continued)
 The use of leucite-reinforced glass ceramic
has declined because of the introduction of
lithium disilicate glass ceramics with improved
mechanical properties.
3.2. Lithium disilicate glass-ceramics
 Second generation.
 In 1998.
 Example: IPS Empress 2 (Ivoclar Vivadent).
 Lithium disilicate crystals: About 65 vol%
dispersed in a glassy matrix.
Lithium disilicate crowns (IPS Empress 2).
3.2. Lithium disilicate glass-ceramics
(continued)
 Porosity: about 1 vol%.
 A glass-ceramic ingot is plasticized at 920°C
and pressed into an investment mold under
vacuum and pressure.
 Their strength is more than twice that of
leucite-reinforced all-ceramics.
 Flexural strength: about 300 MPa.
3.2. Lithium disilicate glass-ceramics
(continued)
 Veneered with fluoroapatite-based porcelain
(IPS Eris; Ivoclar Vivadent).
 Indication: 3-unit FPD in the anterior area, and
can extend to the second premolar.
Microstructure of heat-pressed lithium disilicate glass-ceramic.
IPS e.max Press (Ivoclar Vivadent)
 A newly pressable lithium disilicate glass ceramic.
 In 2005.
 Improved mechanical properties (flexural strength:
440 MPa) and translucency.
 Indications: * Inlays, onlays, and monolithic (full
contour) anterior crowns.
* A core material for crowns and 3-
unit FPD in the anterior region.
4. Glass-infiltrated ceramics
(slip-cast ceramics)
 In the 1990s.
 Condensation of a porcelain slip on a porous
refractory die, which absorbs water from the slip
by capillary action.
 After sintering, the refractory die shrinks more
than the slip. This allows easy separation.
4. Glass-infiltrated ceramics
(continued)
 The sintered porous slip is later infiltrated with a
lanthanum-containing glass, producing two
interpenetrating networks.
 Advantage: higher strength than heat-pressed.
 Disadvantage: long processing times.
4. Glass-infiltrated ceramics
(continued)
Types
4.1. In-Ceram Alumina
4.2. In-Ceram Spinel
4.3. In-Ceram Zirconia
4.1. In-Ceram Alumina (VITA Zahnfabrik)
 In 1989.
 Alumina: 68 vol %, glass: 27 vol %
and porosity: 5 vol %.
 A slurry of densely packed (70–80 wt%) Al2O3
is applied.
Note: slurry means a thick mixture of water and
another substance.
4.1. In-Ceram Alumina
(continued)
 Drying at 120°C for 6 hours.
 Sintered at 1120°C for 2 hours and 1180°C for 2
hours.
 The porous slip is infiltrated with lanthanum glass
at 1100°C for 2 hours to eliminate porosity and
increase strength.
4.1. In-Ceram Alumina
(continued)
 The presence of alumina crystals with a high
refractive index and 5% porosity account for
some degree of opacity.
 Flexural strength: about 550 MPa.
 The core is veneered with feldspathic porcelain.
 Indications: the first all-ceramic system available
for crowns and 3-unit anterior FPDs.
Microstructure of alumina slip-cast ceramic.
4.2. In-Ceram Spinel
 In 1994.
 Mixture of magnesia and alumina (MgAl2O4).
 Better translucency, similar to that of lithium
disilicate heat-pressed ceramics, at the expense
of mechanical properties.
4.2. In-Ceram Spinel
(continued)
 Flexural strength: 350–400 MPa.
 Indication: only recommended for anterior
crowns.
4.3. In-Ceram Zirconia (VITA Zahnfabrik)
 Alumina: 34 vol%.
 zirconia stabilized with 12 mol% ceria (12Ce-
TZP): 33 vol%.
 Glass phase: 23 vol%.
 Porosity: about 8 vol%.
4.3. In-Ceram Zirconia
(continued)
 Highest flexural strength and fracture toughness
of all slip-cast ceramics.
 Flexural strength: about 650 MPa.
 Two types of strengthening mechanisms:
(1) Zirconia stress-induced transformation
toughening.
(2) Alumina crack deflection.
Microstructure of zirconia-toughened alumina slip-cast ceramic.
A: alumina grains, Z: zirconia grains, Arrow indicates pore.
4.3. In-Ceram Zirconia
(continued)
 The core is veneered with feldspathic porcelain.
 Indications: posterior crown and FPD framework.
 Containdication: anterior regions, since the core
is opaque.
5. Machined ceramics
Types
5.1. Computer aided design/computer aided
machining (CAD/CAM) [CEREC system]
5.2. Copy milling [Celay system]
CEREC AC, Sirona Dental System
5.1. CAD/CAM (CEREC system)
 In the early 1970s.
 Types: 5.1.1. Hard machining
5.1.2. Soft machining
 The abutment or die is first scanned.
 The computer software designs the restoration.
 Then, milling the ceramic block by a computer-
aided machine.
5.1.1. Hard machining
 For fully sintered ceramic blocks.
 Final dimensions of the frameworks can be
milled directly.
 Advantages
* Superior fit (in comparison to soft machining),
because no shrinkage is involved in the process.
* Produce restorations in one visit.
5.1.2 Soft machining
 For partially sintered ceramic blocks, followed
by sintering at high temperature.
 In 2001.
 Enlarged frameworks (about 25%) are milled to
compensate for sintering shrinkage.
5.1.2 Soft machining
(continued)
 Advantages: - Easy to mill.
- Save time and tool wear.
 Disadvantage: the benefit of fabricating the
restoration in one visit is lost,
because it requires sintering
after machining.
 Indications: ceramics difficult to machine such
as alumina and zirconia.
5.2. Copy milling [Celay system]
 Milled restorations by duplicating a resin
pattern using a pantographic device similar to
those used for duplicating house keys.
 Unable to approach the sophistication of the
digital systems (CEREC 3D; Sirona Dental
Systems), the Celay system is now obsolete.
Types Subtypes Flexural strength
(Mpa)
Uses
1. Sintered
(not available)
Alumina-based 140 Replaced by heat pressed or
machined all-ceramic restorations
Leucite-reinforced 104
2. Castable
(not available)
150 Not available
3. Heat-
pressed
Leucite-reinforced 150 Inlays, onlays, veneers and
anterior crowns
Lithium disilicate 300 3-unit anterior FPDs, and can
extend to the second premolar
4. Glass-
infiltrated
(slip-cast)
In-Ceram Spinel 350–400 Only recommended for anterior
crowns
In-Ceram Alumina 550 Crowns and 3-unit anterior FPDs
In-Ceram Zirconia 650 Posterior crowns and FPDs
5. Machinable
(CAD/CAM) 3Y-TZP 900–1200
- Crowns & FPDs.
- Orthodontic brackets.
- Endodontic posts.
- Implants and implant abutments.
All-ceramic materials
CAD/CAM ceramics
(Part two)
2017
 All-ceramic restorations can be fabricated by both
traditional laboratory methods and CAD/CAM.
 The traditional laboratory methods
* Time consuming.
* Technique sensitive.
* Unpredictable.
* Could not process high strength polycrystalline
ceramics such as partially stabilized zirconia.
CAD/CAM
 Reduce the fabrication time.
 A good alternative for both the dentists and
laboratories.
 Industrially fabricated blocks are more
homogenous with minimal flaws.
 Can be used for fabrication of both all-ceramic
and the veneering porcelain.
Types of CAD/CAM ceramics
1. CAD/CAM with feldspathic ceramics
2. CAD/CAM with mica-based ceramics
3. CAD/CAM with leucite-reinforced ceramics
4. CAD/CAM with lithium disilicate reinforced
ceramics
5. CAD/CAM with glass-infiltrated alumina and
zirconia ceramics
6. CAD/CAM with polycrystalline alumina and
zirconia
6.1. Alumina-based polycrystalline ceramics
6.2. Stabilized zirconia-based polycrystalline
ceramics
6.2.1. Yttria partially stabilized tetragonal
zirconia polycrystals (3Y-TZP)
6.2.2. Magnesia partially stabilized zirconia
6.2.3. Ceria stabilized zirconia/alumina
nanocomposite (Ce-TZP/A)
1. CAD/CAM with feldspathic ceramics
 Feldspar (Na,K Al Si3O8) as a major
crystalline phase: 30 vol%.
 Flexural strength: 120 MPa.
 Excellent aesthetic properties
 Indications: veneers, inlays, onlays and
anterior crowns.
1. CAD/CAM with feldspathic ceramics
(Continued)
1.1. VitaTM Mark I (Vita Zahnfabrik)
 In 1985.
 The first CAD/CAM produced inlay & onlay.
 Fine grain feldspathic ceramic block.
 Fully sintered for hard machining.
1. CAD/CAM with feldspathic ceramics
(Continued)
1.2. VitaTM Mark II (Vita Zahnfabrik)
 In 1991.
 Better mechanical properties.
 Flexural strength: 100–160 Mpa.
 Made of materials similar to conventional
feldspathic ceramic.
2. CAD/CAM with mica-based ceramics
 Example: DicorTM MGC.
 Mica crystals: 70%.
 Flexural strength: about 229 MPa.
 Cumulative breakage at 2 years was higher
than for VitaTM Mark II.
 No longer in the market.
3. CAD/CAM with leucite-reinforced ceramics
 Similar in microstructure and mechanical
properties to the first generation heat pressed
leucite-reinforced ceramics.
3.1. ProCAD (Ivoclar-Vivadent).
 In 1998.
 Similar in structure, marginal gap and fracture
load to the heat-pressed ceramic EmpressTM
(Ivoclar-Vivadent).
Before and after treatment with all-ceramic restorations (lithium disilicate
IPS e.max Press Tooth 24 inlay; onlays 26, 27; and crowns14, 15, 25)
and CAD/CAM-fabricated leucite ProCAD onlay 16, 26.
3. CAD/CAM with leucite-reinforced ceramics
(continued)
3.2. EmpressTM CAD (Ivoclar-Vivadent)
 In 2006.
 Leucite crystals: about 45%.
 Finer particle size of about 1–5 μm that helps
resist machining damages.
 The powder is first pressed into blocks and
then sintered.
3.2. EmpressTM CAD (continued)
 Flexural strength: about 160 MPa.
 Indication: chair-side single unit restorations.
 Available in:
- High Translucency (EmpressTM CAD HT)
- Low Translucency (EmpressTM CAD LT)
- Polychromatic (EmpressTM CAD Multi)
 The milled restoration can be stained and
glazed.
4. CAD/CAM with lithium disilicate
reinforced ceramics
 Example: IPSTM e.max CAD (Ivoclar-Vivadent).
 In 2006.
 Fully sintered, but partially crystallized.
 The block exhibits a flexural strength of 130–
150 MPa in the pre-crystallized (blue) state.
 Allows simplified machining and intraoral
occlusal adjustment.
4. CAD/CAM with lithium disilicate
reinforced ceramics (continued)
 Crystallize in a chair-side ceramic oven at 850°C
in vacuum for 20–25 min, and changes from blue
to the selected shade.
 Lithium disilicate crystals: 70 vol%.
 Final flexural strength: 300–360 MPa.
 Indication: - Chair-side monolithic (full anatomic)
anterior and posterior crowns.
- Inlay, onlay, and veneer.
5. CAD/CAM with glass-infiltrated ceramics
 In 1993.
 Presintered blocks to fabricate copings which are
further glass-infiltrated.
5.1. CAD/ CAM InCeramTM Spinell
 The most translucent of this group .
 Flexural strength: 350 MPa.
 Indication: anterior crowns.
5.2. CAD/CAM InCeramTM Alumina
 Flexural strength: 450–600 MPa.
 Marginal gap: 70 μm (clinically acceptable).
 Indications: - Anterior and posterior crowns.
- 3-unit anterior FPD.
5.3. CAD/CAM InCeramTM Zirconia
 Flexural strength: 700 MPa.
 Better fit than the slip cast InCeramTM Zirconia.
 Indications: the opacity of zirconia has limited
its use to the posterior crowns and
FPDs.
6. CAD/CAM with polycrystalline
alumina and zirconia
 Polycrystalline ceramics, such as alumina and
zirconia, have no intervening etchable glassy
matrix.
 The crystals are densely packed, and then
sintered.
 The dense crystal lattice reduces crack
propagation resulting in excellent mechanical
properties.
 Indications: crown and bridge copings.
6.1. Alumina-based polycrystalline ceramics
 Example: ProceraTM AllCeram (Nobel Biocare).
 The first fully dense dental polycrystalline
ceramic.
 In 1993.
 More than 99.9% alumina.
 Computer-aided production of enlarged die
(20%) to compensate for the sintering
shrinkage.
6.1. Alumina-based polycrystalline ceramics
(continued)
 Alumina is densely packed (dry pressed) and
then sintered at 1550°C.
 Flexural strength: about 600 MPa.
 The highest strength of the alumina-based
materials, but lower than zirconia.
 The highest elastic modulus and hardness of all-
ceramic materials.
6.1. Alumina-based polycrystalline ceramics
(continued)
 Veneered with matched expansion porcelain.
 Marginal fit: 70 μm (within the range of clinical
acceptance).
 Indications: - Veneers.
- Crowns.
- Anterior FPDs.
6.2. Stabilized zirconia-based
polycrystalline ceramics
Introduction
Advantages of zirconia
 High biocompatibility.
 High strength and fracture toughness.
 Low bacterial surface adhesion
 Low thermal conductivity.
 Low corrosion potential.
 Good radiopacity.
 Zirconia is a polymorphic material.
 It has three crystallographic forms:
* Monoclinic (M): from room temperature to
1170°C.
* Tetragonal (T): from 1170°C to 2370°C.
* Cubic (C): from 2370°C to the melting point
(2715°C).
 With the addition of stabilizing oxides such as
ceria (CeO2), magnesia (MgO) or yttria (Y2O3),
a partially stabilized zirconia (PSZ) is formed
at room temperature with cubic crystals as the
major phase, and monoclinic and tetragonal
crystals as the minor phases.
 It is also possible to form a mono-phasic
material consisting of tetragonal crystals only,
and the material is called tetragonal zirconia
polycrystal (TZP).
Transformation toughening of zirconia
 Stress at the crack tip will trigger transformation
from tetragonal to monoclinic phase (T–M
transformation).
 Accompanied by an increase in volume (about
4.5%) as monoclinic crystals are larger in size.
 Induce compressive stress at the crack tip.
 Hinder (not totally prevent) the crack propagation.
 Resulting in an increase in mechanical properties.
 Zirconia has:
- High fracture toughness: 9–10 MPa m-1
- High Flexural strength: 900–1200 Mpa
(about twice that of alumina).
Low temperature degradation (LTD) of zirconia
 Progressive spontaneous slow transformation
of the metastable tetragonal phase into the
monoclinic phase in the presence of water at
relatively low temperatures (150–400°C).
 Yttria reacts with water vapor to form yttrium
hydroxide, resulting in instability of the
tetragonal zirconia.
 LTD initiates at the surface and subsequently
progresses into the bulk of the material.
 Accompanied by an increase in volume, which
causes stress and microcracking.
 Microcracking results in:
* Grain pullout.
* Surface roughness.
* Water penetration.
* Decrease in strength (strength degradation).
 Factors affecting LTD
* Stabilizer type, concentration and distribution.
* Grain size.
* Residual stresses.
 Above a critical grain size, 3Y-TZP is less
stable and more susceptible to spontaneous
transformation.
 Smaller grain sizes are associated with a lower
transformation rate.
 Higher sintering temperature and time lead to:
- Larger grain size.
- Higher translucency.
- More susceptible to transformation and LTD.
Scanning electron micrographs showing the effect of sintering temperature on
grain size in 3Y-TZP sintered for 2 hr. (A) 1,300°C; (B) 1,350°C; (C) 1,400°C;
(D) 1,450°C; (E) 1,500°C; (F) 1,550°C; (G) 1,600°C; and (H) 1,650°C.
 Although some concern was raised by the
degradation of femoral heads 20 years ago, no
direct correlation has been established between
LTD and clinical failure of zirconia in dentistry.
6.2.1. Yttria partially stabilized tetragonal
zirconia polycrystals (3Y-TZP)
 Yttria: 3 mol%.
 Radiopacity is comparable to metal.
 Applications
- Crowns & FPDs.
- Orthodontic brackets.
- Endodontic posts.
- Implants and implant abutments.
- Its use in the esthetic zone is limited to the
fabrication of frameworks.
3Y-TZP (continued)
 Colored zirconia frameworks are now available,
and produce a more clinically acceptable color
match.
 Examples for partially sintered blanks
- LAVATM (3M ESPE).
- CerconTM (Dentsply).
- e.maxTM ZirCAD (Ivoclar-Vivadent).
- ProceraTM Zirconia (NobelBiocare).
- VitaTM YZ blocks (Vita Zahnfabrik).
3Y-TZP (continued)
 Examples for fully sintered zirconia blocks: DC
ZirkonTM (Smartfit Austenal).
 Milling the softer partially sintered blanks (green
state): - Shortens the milling time.
- Reduces the wear of milling tools.
 Soft machining of dental restorations requires
sintering at 1350–1550°C for 2–6 hours.
3Y-TZP (continued)
 Porosity after sintering: less than 0.5 vol%.
 Flexural strength: 900–1200 MPa.
 Fracture toughness: 9–10 MPa.m0.5
 Fully sintered Y-TZP blocks have been processed
by hot isostatic pressing.
Note: isostatic means equal pressure from every
side.
3Y-TZP (continued)
 Because of the hardness and poor machinability
of fully sintered Y-TZP, a robust milling system
and extended milling periods are required.
 Milling fully sintered zirconia may compromise the
microstructure and strength of the material.
6.2.2. Magnesium partially stabilized
zirconia (Mg-PSZ)
 Magnesia: 8–10 mol%.
 Tetragonal crystals in a cubic matrix.
 Decreased stability of the tetragonal phase in a
wet environment when compared to 3Y-TZP
after veneering.
Mg-PSZ (continued)
 Lower mechanical properties.
 Porosity and large grain size has limited its
success.
 Example: Denzir-MTM (Dentronic) for hard
machining.
6.2.3. Ceria stabilized zirconia/alumina
nanocomposite (Ce-TZP/A)
 Example: NANOZR.
 Alumina: 30 vol%.
 Ceria: 10 mol%.
 Alumina nanoparticles (10–100 nm) are trapped
within zirconia grains,
and zirconia nanoparticles (10 nm) are trapped
within alumina grains.
Microstructure of a conventional Y-TZP (left) and
a Ce-TZP/alumina nanocomposite (right).
Ce-TZP/A (continued)
 Excellent resistance to LTD.
 Better mechanical properties than Y-TZP.
 Highest flexural strength: about 1400 MPa.
 Highest fracture toughness: 19 MPa.m0.5.
 Reliable framework for posterior FPDs.
Inhibition of crack propagation by stress-induced
phase transformation.
All-ceramic presentation powerpoint 2 parts

More Related Content

What's hot

Pressable ceramics
Pressable ceramicsPressable ceramics
Pressable ceramics
Dr.shifaya nasrin
 
Ceramics strengthening techniques
Ceramics strengthening techniquesCeramics strengthening techniques
Ceramics strengthening techniques
Radwa Eldessouky
 

What's hot (20)

Pressable ceramics
Pressable ceramicsPressable ceramics
Pressable ceramics
 
DENTAL CERAMICS
DENTAL CERAMICSDENTAL CERAMICS
DENTAL CERAMICS
 
advances in resin composites dental material
 advances in resin composites dental material advances in resin composites dental material
advances in resin composites dental material
 
METAL FREE CERAMICS- AN UPDATE
METAL FREE CERAMICS- AN UPDATEMETAL FREE CERAMICS- AN UPDATE
METAL FREE CERAMICS- AN UPDATE
 
Ceramics strengthening techniques
Ceramics strengthening techniquesCeramics strengthening techniques
Ceramics strengthening techniques
 
Dental ceramics
Dental ceramicsDental ceramics
Dental ceramics
 
Ceramics seminar
Ceramics seminarCeramics seminar
Ceramics seminar
 
Recent Advances in Dental Ceramics
Recent Advances in Dental CeramicsRecent Advances in Dental Ceramics
Recent Advances in Dental Ceramics
 
Ceramic restorations
Ceramic restorationsCeramic restorations
Ceramic restorations
 
Dental cast base metal alloys (2)
Dental cast base metal alloys (2)Dental cast base metal alloys (2)
Dental cast base metal alloys (2)
 
Dental ceramics part 2
Dental ceramics part 2 Dental ceramics part 2
Dental ceramics part 2
 
Porcelain
PorcelainPorcelain
Porcelain
 
Classification of dental porcelain / dental courses
Classification of dental porcelain / dental coursesClassification of dental porcelain / dental courses
Classification of dental porcelain / dental courses
 
Ceramic2
Ceramic2Ceramic2
Ceramic2
 
DENTAL CERAMICS AN INTRODUCTION
DENTAL CERAMICS AN INTRODUCTIONDENTAL CERAMICS AN INTRODUCTION
DENTAL CERAMICS AN INTRODUCTION
 
Resin based composites(Recent Advances)
Resin based composites(Recent Advances)Resin based composites(Recent Advances)
Resin based composites(Recent Advances)
 
Dental Ceramics and Porcelain fused to metal
Dental Ceramics and Porcelain fused to metal Dental Ceramics and Porcelain fused to metal
Dental Ceramics and Porcelain fused to metal
 
Dental casting alloys
Dental casting alloysDental casting alloys
Dental casting alloys
 
all ceramic restoration
all ceramic restorationall ceramic restoration
all ceramic restoration
 
Zirconia
ZirconiaZirconia
Zirconia
 

Similar to All-ceramic presentation powerpoint 2 parts

Similar to All-ceramic presentation powerpoint 2 parts (20)

ALL CERAMIC RESTORATIONS-Dr MEENU MERRY C PAUL
ALL CERAMIC RESTORATIONS-Dr MEENU MERRY C PAULALL CERAMIC RESTORATIONS-Dr MEENU MERRY C PAUL
ALL CERAMIC RESTORATIONS-Dr MEENU MERRY C PAUL
 
Dental ceramics part II
Dental ceramics part IIDental ceramics part II
Dental ceramics part II
 
All Ceramic Materials.pptx
All Ceramic Materials.pptxAll Ceramic Materials.pptx
All Ceramic Materials.pptx
 
Introduction to ceramics
Introduction to ceramics Introduction to ceramics
Introduction to ceramics
 
Evolution of all ceramics&amp;recent advances (2)/ dental courses
Evolution of all ceramics&amp;recent advances (2)/ dental coursesEvolution of all ceramics&amp;recent advances (2)/ dental courses
Evolution of all ceramics&amp;recent advances (2)/ dental courses
 
Introduction to ceramics menna
Introduction to ceramics mennaIntroduction to ceramics menna
Introduction to ceramics menna
 
Dental Ceramics.. old and new.
Dental Ceramics.. old and new.Dental Ceramics.. old and new.
Dental Ceramics.. old and new.
 
Classification of porcelain / dental implant companies
Classification of porcelain / dental implant companiesClassification of porcelain / dental implant companies
Classification of porcelain / dental implant companies
 
Ceramics Industry.ppt
Ceramics Industry.pptCeramics Industry.ppt
Ceramics Industry.ppt
 
Evolution of Dental ceramic restorations /certified fixed orthodontic course...
 Evolution of Dental ceramic restorations /certified fixed orthodontic course... Evolution of Dental ceramic restorations /certified fixed orthodontic course...
Evolution of Dental ceramic restorations /certified fixed orthodontic course...
 
Evolution of all ceramics&recent advances (2)
Evolution of all ceramics&recent advances (2)Evolution of all ceramics&recent advances (2)
Evolution of all ceramics&recent advances (2)
 
All ceramics /fixed orthodontic training
All ceramics /fixed orthodontic trainingAll ceramics /fixed orthodontic training
All ceramics /fixed orthodontic training
 
Ceramics1
Ceramics1Ceramics1
Ceramics1
 
Ceramic 2
Ceramic 2Ceramic 2
Ceramic 2
 
Ceramic 2
Ceramic 2Ceramic 2
Ceramic 2
 
Phy351 ch 7
Phy351 ch 7Phy351 ch 7
Phy351 ch 7
 
Ceramics
CeramicsCeramics
Ceramics
 
Fayza ceramics
Fayza ceramicsFayza ceramics
Fayza ceramics
 
introduction to ceramics
introduction to   ceramicsintroduction to   ceramics
introduction to ceramics
 
Structural ceramics
Structural ceramics Structural ceramics
Structural ceramics
 

More from Ahmed Mostafa Hussein Mohammed

More from Ahmed Mostafa Hussein Mohammed (17)

Recent dental composite resins
 Recent  dental composite resins Recent  dental composite resins
Recent dental composite resins
 
Impression materials part 2
Impression materials part 2Impression materials part 2
Impression materials part 2
 
Impression materials part 1
Impression materials part 1 Impression materials part 1
Impression materials part 1
 
Resin luting cements (Word)
Resin luting cements (Word)Resin luting cements (Word)
Resin luting cements (Word)
 
Resin Luting Cements (2nd edition) pdf
Resin Luting Cements (2nd edition) pdfResin Luting Cements (2nd edition) pdf
Resin Luting Cements (2nd edition) pdf
 
Resin Luting cements (2nd edition)
Resin Luting cements (2nd edition) Resin Luting cements (2nd edition)
Resin Luting cements (2nd edition)
 
Calcium phosphate bone cement word
Calcium phosphate bone cement wordCalcium phosphate bone cement word
Calcium phosphate bone cement word
 
Calcium phosphate bone cement presentation
Calcium phosphate bone cement  presentationCalcium phosphate bone cement  presentation
Calcium phosphate bone cement presentation
 
Synthesis of silver nanoparticles presentation
Synthesis of silver nanoparticles presentation Synthesis of silver nanoparticles presentation
Synthesis of silver nanoparticles presentation
 
Synthesis of hydroxyapatite nanoparticles
Synthesis of hydroxyapatite nanoparticlesSynthesis of hydroxyapatite nanoparticles
Synthesis of hydroxyapatite nanoparticles
 
Irrigation techniques
Irrigation techniques Irrigation techniques
Irrigation techniques
 
Intracanal medicaments
Intracanal medicaments Intracanal medicaments
Intracanal medicaments
 
Irrigants in endodontics
Irrigants in endodontics Irrigants in endodontics
Irrigants in endodontics
 
Flexible resin denture presentation power point
Flexible resin denture presentation power pointFlexible resin denture presentation power point
Flexible resin denture presentation power point
 
Flexible resin denture word
Flexible resin denture  wordFlexible resin denture  word
Flexible resin denture word
 
Apexification apexogenesis MTA mineral trioxide aggregate powerpoint prese...
Apexification  apexogenesis  MTA  mineral trioxide aggregate powerpoint prese...Apexification  apexogenesis  MTA  mineral trioxide aggregate powerpoint prese...
Apexification apexogenesis MTA mineral trioxide aggregate powerpoint prese...
 
Apexification apeogenesis word2007 MTA mineral trioxide aggregate
Apexification apeogenesis word2007 MTA mineral trioxide aggregateApexification apeogenesis word2007 MTA mineral trioxide aggregate
Apexification apeogenesis word2007 MTA mineral trioxide aggregate
 

Recently uploaded

Call Girl in Chennai | Whatsapp No 📞 7427069034 📞 VIP Escorts Service Availab...
Call Girl in Chennai | Whatsapp No 📞 7427069034 📞 VIP Escorts Service Availab...Call Girl in Chennai | Whatsapp No 📞 7427069034 📞 VIP Escorts Service Availab...
Call Girl in Chennai | Whatsapp No 📞 7427069034 📞 VIP Escorts Service Availab...
amritaverma53
 
Kolkata Call Girls Service ❤️🍑 9xx000xx09 👄🫦 Independent Escort Service Kolka...
Kolkata Call Girls Service ❤️🍑 9xx000xx09 👄🫦 Independent Escort Service Kolka...Kolkata Call Girls Service ❤️🍑 9xx000xx09 👄🫦 Independent Escort Service Kolka...
Kolkata Call Girls Service ❤️🍑 9xx000xx09 👄🫦 Independent Escort Service Kolka...
Sheetaleventcompany
 
Premium Call Girls Nagpur {9xx000xx09} ❤️VVIP POOJA Call Girls in Nagpur Maha...
Premium Call Girls Nagpur {9xx000xx09} ❤️VVIP POOJA Call Girls in Nagpur Maha...Premium Call Girls Nagpur {9xx000xx09} ❤️VVIP POOJA Call Girls in Nagpur Maha...
Premium Call Girls Nagpur {9xx000xx09} ❤️VVIP POOJA Call Girls in Nagpur Maha...
Sheetaleventcompany
 

Recently uploaded (20)

ANATOMY AND PHYSIOLOGY OF REPRODUCTIVE SYSTEM.pptx
ANATOMY AND PHYSIOLOGY OF REPRODUCTIVE SYSTEM.pptxANATOMY AND PHYSIOLOGY OF REPRODUCTIVE SYSTEM.pptx
ANATOMY AND PHYSIOLOGY OF REPRODUCTIVE SYSTEM.pptx
 
7 steps How to prevent Thalassemia : Dr Sharda Jain & Vandana Gupta
7 steps How to prevent Thalassemia : Dr Sharda Jain & Vandana Gupta7 steps How to prevent Thalassemia : Dr Sharda Jain & Vandana Gupta
7 steps How to prevent Thalassemia : Dr Sharda Jain & Vandana Gupta
 
Call Girl In Chandigarh 📞9809698092📞 Just📲 Call Inaaya Chandigarh Call Girls ...
Call Girl In Chandigarh 📞9809698092📞 Just📲 Call Inaaya Chandigarh Call Girls ...Call Girl In Chandigarh 📞9809698092📞 Just📲 Call Inaaya Chandigarh Call Girls ...
Call Girl In Chandigarh 📞9809698092📞 Just📲 Call Inaaya Chandigarh Call Girls ...
 
Exclusive Call Girls Bangalore {7304373326} ❤️VVIP POOJA Call Girls in Bangal...
Exclusive Call Girls Bangalore {7304373326} ❤️VVIP POOJA Call Girls in Bangal...Exclusive Call Girls Bangalore {7304373326} ❤️VVIP POOJA Call Girls in Bangal...
Exclusive Call Girls Bangalore {7304373326} ❤️VVIP POOJA Call Girls in Bangal...
 
Call Girls Bangalore - 450+ Call Girl Cash Payment 💯Call Us 🔝 6378878445 🔝 💃 ...
Call Girls Bangalore - 450+ Call Girl Cash Payment 💯Call Us 🔝 6378878445 🔝 💃 ...Call Girls Bangalore - 450+ Call Girl Cash Payment 💯Call Us 🔝 6378878445 🔝 💃 ...
Call Girls Bangalore - 450+ Call Girl Cash Payment 💯Call Us 🔝 6378878445 🔝 💃 ...
 
Call Girl in Chennai | Whatsapp No 📞 7427069034 📞 VIP Escorts Service Availab...
Call Girl in Chennai | Whatsapp No 📞 7427069034 📞 VIP Escorts Service Availab...Call Girl in Chennai | Whatsapp No 📞 7427069034 📞 VIP Escorts Service Availab...
Call Girl in Chennai | Whatsapp No 📞 7427069034 📞 VIP Escorts Service Availab...
 
Call 8250092165 Patna Call Girls ₹4.5k Cash Payment With Room Delivery
Call 8250092165 Patna Call Girls ₹4.5k Cash Payment With Room DeliveryCall 8250092165 Patna Call Girls ₹4.5k Cash Payment With Room Delivery
Call 8250092165 Patna Call Girls ₹4.5k Cash Payment With Room Delivery
 
❤️Chandigarh Escorts Service☎️9814379184☎️ Call Girl service in Chandigarh☎️ ...
❤️Chandigarh Escorts Service☎️9814379184☎️ Call Girl service in Chandigarh☎️ ...❤️Chandigarh Escorts Service☎️9814379184☎️ Call Girl service in Chandigarh☎️ ...
❤️Chandigarh Escorts Service☎️9814379184☎️ Call Girl service in Chandigarh☎️ ...
 
Ahmedabad Call Girls Book Now 9630942363 Top Class Ahmedabad Escort Service A...
Ahmedabad Call Girls Book Now 9630942363 Top Class Ahmedabad Escort Service A...Ahmedabad Call Girls Book Now 9630942363 Top Class Ahmedabad Escort Service A...
Ahmedabad Call Girls Book Now 9630942363 Top Class Ahmedabad Escort Service A...
 
Kolkata Call Girls Service ❤️🍑 9xx000xx09 👄🫦 Independent Escort Service Kolka...
Kolkata Call Girls Service ❤️🍑 9xx000xx09 👄🫦 Independent Escort Service Kolka...Kolkata Call Girls Service ❤️🍑 9xx000xx09 👄🫦 Independent Escort Service Kolka...
Kolkata Call Girls Service ❤️🍑 9xx000xx09 👄🫦 Independent Escort Service Kolka...
 
Race Course Road } Book Call Girls in Bangalore | Whatsapp No 6378878445 VIP ...
Race Course Road } Book Call Girls in Bangalore | Whatsapp No 6378878445 VIP ...Race Course Road } Book Call Girls in Bangalore | Whatsapp No 6378878445 VIP ...
Race Course Road } Book Call Girls in Bangalore | Whatsapp No 6378878445 VIP ...
 
Kolkata Call Girls Shobhabazar 💯Call Us 🔝 8005736733 🔝 💃 Top Class Call Gir...
Kolkata Call Girls Shobhabazar  💯Call Us 🔝 8005736733 🔝 💃  Top Class Call Gir...Kolkata Call Girls Shobhabazar  💯Call Us 🔝 8005736733 🔝 💃  Top Class Call Gir...
Kolkata Call Girls Shobhabazar 💯Call Us 🔝 8005736733 🔝 💃 Top Class Call Gir...
 
Premium Call Girls Nagpur {9xx000xx09} ❤️VVIP POOJA Call Girls in Nagpur Maha...
Premium Call Girls Nagpur {9xx000xx09} ❤️VVIP POOJA Call Girls in Nagpur Maha...Premium Call Girls Nagpur {9xx000xx09} ❤️VVIP POOJA Call Girls in Nagpur Maha...
Premium Call Girls Nagpur {9xx000xx09} ❤️VVIP POOJA Call Girls in Nagpur Maha...
 
Cardiac Output, Venous Return, and Their Regulation
Cardiac Output, Venous Return, and Their RegulationCardiac Output, Venous Return, and Their Regulation
Cardiac Output, Venous Return, and Their Regulation
 
Call Girls Rishikesh Just Call 9667172968 Top Class Call Girl Service Available
Call Girls Rishikesh Just Call 9667172968 Top Class Call Girl Service AvailableCall Girls Rishikesh Just Call 9667172968 Top Class Call Girl Service Available
Call Girls Rishikesh Just Call 9667172968 Top Class Call Girl Service Available
 
💰Call Girl In Bangalore☎️7304373326💰 Call Girl service in Bangalore☎️Bangalor...
💰Call Girl In Bangalore☎️7304373326💰 Call Girl service in Bangalore☎️Bangalor...💰Call Girl In Bangalore☎️7304373326💰 Call Girl service in Bangalore☎️Bangalor...
💰Call Girl In Bangalore☎️7304373326💰 Call Girl service in Bangalore☎️Bangalor...
 
Call Girls Kathua Just Call 8250077686 Top Class Call Girl Service Available
Call Girls Kathua Just Call 8250077686 Top Class Call Girl Service AvailableCall Girls Kathua Just Call 8250077686 Top Class Call Girl Service Available
Call Girls Kathua Just Call 8250077686 Top Class Call Girl Service Available
 
ANATOMY AND PHYSIOLOGY OF RESPIRATORY SYSTEM.pptx
ANATOMY AND PHYSIOLOGY OF RESPIRATORY SYSTEM.pptxANATOMY AND PHYSIOLOGY OF RESPIRATORY SYSTEM.pptx
ANATOMY AND PHYSIOLOGY OF RESPIRATORY SYSTEM.pptx
 
(RIYA)🎄Airhostess Call Girl Jaipur Call Now 8445551418 Premium Collection Of ...
(RIYA)🎄Airhostess Call Girl Jaipur Call Now 8445551418 Premium Collection Of ...(RIYA)🎄Airhostess Call Girl Jaipur Call Now 8445551418 Premium Collection Of ...
(RIYA)🎄Airhostess Call Girl Jaipur Call Now 8445551418 Premium Collection Of ...
 
❤️Call Girl Service In Chandigarh☎️9814379184☎️ Call Girl in Chandigarh☎️ Cha...
❤️Call Girl Service In Chandigarh☎️9814379184☎️ Call Girl in Chandigarh☎️ Cha...❤️Call Girl Service In Chandigarh☎️9814379184☎️ Call Girl in Chandigarh☎️ Cha...
❤️Call Girl Service In Chandigarh☎️9814379184☎️ Call Girl in Chandigarh☎️ Cha...
 

All-ceramic presentation powerpoint 2 parts

  • 2.  All-ceramics contain a large amount of crystalline phase (35–99 vol%), which is responsible for improving mechanical properties.
  • 3. Types of all-ceramic materials 1. Sintered all-ceramic materials 2. Castable glass ceramics 3. Heat-pressed ceramics 4. Glass-infiltrated ceramics (slip-cast ceramics) 5. Machined ceramics
  • 4. Types Subtypes Crystals percentage 1. Sintered (not available) Alumina-based Alumina 40–50 wt% Leucite-reinforced Leucite 45 vol% 2. Castable (not available) Mica 45% 3. Heat- pressed Leucite-reinforced Leucite 35–45 vol% Lithium disilicate Lithium disilicate 65 vol% 4. Glass- infiltrated (slip-cast) In-Ceram Alumina Alumina 68 vol% In-Ceram Spinel Magnesia & alumina In-Ceram Zirconia Alumina 12Ce-TZP 34 vol% 33 vol% 12Ce-TZP: zirconia stabilized with 12 mol% ceria . All-ceramic materials
  • 5. Translucency Leucite > Lithium disilicate & Magnesia > Alumina > Zirconia-based ceramics. Flexural strength Leucite < Lithium disilicate & Magnesia < Alumina < Zirconia-based ceramics. (150) (300) (350–400) (550–600) (650–1400 Mpa) Highest fracture toughness: zirconia-based ceramics (3Y-TZP & Ce-TZP/A).  3Y-TZP: Yttria partially stabilized tetragonal zirconia polycrystals.  Ce-TZP/A: ceria stabilized zirconia/alumina nanocomposite . Highest elastic modulus: alumina-based ceramics (Procera).
  • 6. 1. Sintered all-ceramic materials Types 1.1. Alumina-based ceramics 1.2. Leucite-reinforced ceramics
  • 8. 1.1. Alumina-based ceramics  By McLean in 1965.  Alumina crystals: 40–50% by weight.  Flexural strength: about 140 MPa (about twice that of feldspathic porcelain).
  • 9. 1.1. Alumina-based ceramics (continued)  Higher elastic modulus and fracture toughness compared to feldspathic porcelain.  Veneered with matched-expansion porcelain.
  • 10. 1.2. Leucite-reinforced ceramics * Leucite crystals: up to 45 vol%. * Flexural strength: 104 MPa. * High thermal contraction coefficient.
  • 11. 1.2. Leucite-reinforced ceramics (continued)  Large mismatch in thermal contraction between leucite crystals and glass matrix results in tangential compressive stresses in the glass around leucite crystals.  These stresses act as crack deflectors and increase the resistance to crack propagation.
  • 12. Note: Sintered all-ceramic restorations are now being replaced by heat pressed or machined all- ceramic restorations.
  • 13. 2. Castable glass ceramics  In 1980s.  Example: Dicor (Dentsply).  Tetrasilicic fluormica crystals: 45% & glass matrix.
  • 14. 2. Castable glass ceramics (continued)  Made using the lost-wax technique.  Flexural strength: about 150 MPa.  No longer available in the market.
  • 15. 3. Heat-pressed ceramics  In the early 1990s.  Pressed at high temperature (920–1180°C) for 20 min in a phosphate-bonded investment mold produced by the lost-wax technique.  Advantages: * Short processing times. * Good esthetics.
  • 16. 3. Heat-pressed ceramics (continued) Disadvantages  Relatively lower strength compared to alumina and zirconia slip-cast and machinable.  Relatively inexpensive equipments. Types: 3.1. Leucite-reinforced glass ceramics. 3.2. Lithium disilicate glass-ceramics.
  • 19. 3.1. Leucite-reinforced glass ceramics  First generation.  Example: IPS Empress (Ivoclar Vivadent).  Leucite crystals: 35–45 vol% dispersed in a glassy matrix.  Porosity: about 9%.  The molding procedure is conducted at 1080°C for about 20 min.
  • 20. (A) Feldspathic dental porcelain. (B) Leucite-reinforced ceramic.
  • 21. 3.1. Leucite-reinforced glass ceramics (continued)  Tangential compressive stresses develop around the crystals on cooling because of the difference in the coefficient of thermal expansion (CTE) between leucite crystals and the glassy matrix.  These stresses contribute to crack deflection and improved mechanical performance.
  • 22. 3.1. Leucite-reinforced glass ceramics (continued)  Flexural strength and fracture toughness values are about double those of feldspathic porcelains.  Flexural strength: about 150 MPa.  Indications: inlays, onlays, veneers and anterior crowns.
  • 23. 3.1. Leucite-reinforced glass ceramics (continued)  The use of leucite-reinforced glass ceramic has declined because of the introduction of lithium disilicate glass ceramics with improved mechanical properties.
  • 24. 3.2. Lithium disilicate glass-ceramics  Second generation.  In 1998.  Example: IPS Empress 2 (Ivoclar Vivadent).  Lithium disilicate crystals: About 65 vol% dispersed in a glassy matrix.
  • 25. Lithium disilicate crowns (IPS Empress 2).
  • 26. 3.2. Lithium disilicate glass-ceramics (continued)  Porosity: about 1 vol%.  A glass-ceramic ingot is plasticized at 920°C and pressed into an investment mold under vacuum and pressure.  Their strength is more than twice that of leucite-reinforced all-ceramics.  Flexural strength: about 300 MPa.
  • 27. 3.2. Lithium disilicate glass-ceramics (continued)  Veneered with fluoroapatite-based porcelain (IPS Eris; Ivoclar Vivadent).  Indication: 3-unit FPD in the anterior area, and can extend to the second premolar.
  • 28. Microstructure of heat-pressed lithium disilicate glass-ceramic.
  • 29. IPS e.max Press (Ivoclar Vivadent)  A newly pressable lithium disilicate glass ceramic.  In 2005.  Improved mechanical properties (flexural strength: 440 MPa) and translucency.  Indications: * Inlays, onlays, and monolithic (full contour) anterior crowns. * A core material for crowns and 3- unit FPD in the anterior region.
  • 30. 4. Glass-infiltrated ceramics (slip-cast ceramics)  In the 1990s.  Condensation of a porcelain slip on a porous refractory die, which absorbs water from the slip by capillary action.  After sintering, the refractory die shrinks more than the slip. This allows easy separation.
  • 31. 4. Glass-infiltrated ceramics (continued)  The sintered porous slip is later infiltrated with a lanthanum-containing glass, producing two interpenetrating networks.  Advantage: higher strength than heat-pressed.  Disadvantage: long processing times.
  • 32. 4. Glass-infiltrated ceramics (continued) Types 4.1. In-Ceram Alumina 4.2. In-Ceram Spinel 4.3. In-Ceram Zirconia
  • 33. 4.1. In-Ceram Alumina (VITA Zahnfabrik)  In 1989.  Alumina: 68 vol %, glass: 27 vol % and porosity: 5 vol %.  A slurry of densely packed (70–80 wt%) Al2O3 is applied. Note: slurry means a thick mixture of water and another substance.
  • 34. 4.1. In-Ceram Alumina (continued)  Drying at 120°C for 6 hours.  Sintered at 1120°C for 2 hours and 1180°C for 2 hours.  The porous slip is infiltrated with lanthanum glass at 1100°C for 2 hours to eliminate porosity and increase strength.
  • 35. 4.1. In-Ceram Alumina (continued)  The presence of alumina crystals with a high refractive index and 5% porosity account for some degree of opacity.  Flexural strength: about 550 MPa.  The core is veneered with feldspathic porcelain.  Indications: the first all-ceramic system available for crowns and 3-unit anterior FPDs.
  • 36. Microstructure of alumina slip-cast ceramic.
  • 37. 4.2. In-Ceram Spinel  In 1994.  Mixture of magnesia and alumina (MgAl2O4).  Better translucency, similar to that of lithium disilicate heat-pressed ceramics, at the expense of mechanical properties.
  • 38. 4.2. In-Ceram Spinel (continued)  Flexural strength: 350–400 MPa.  Indication: only recommended for anterior crowns.
  • 39. 4.3. In-Ceram Zirconia (VITA Zahnfabrik)  Alumina: 34 vol%.  zirconia stabilized with 12 mol% ceria (12Ce- TZP): 33 vol%.  Glass phase: 23 vol%.  Porosity: about 8 vol%.
  • 40. 4.3. In-Ceram Zirconia (continued)  Highest flexural strength and fracture toughness of all slip-cast ceramics.  Flexural strength: about 650 MPa.  Two types of strengthening mechanisms: (1) Zirconia stress-induced transformation toughening. (2) Alumina crack deflection.
  • 41. Microstructure of zirconia-toughened alumina slip-cast ceramic. A: alumina grains, Z: zirconia grains, Arrow indicates pore.
  • 42. 4.3. In-Ceram Zirconia (continued)  The core is veneered with feldspathic porcelain.  Indications: posterior crown and FPD framework.  Containdication: anterior regions, since the core is opaque.
  • 43. 5. Machined ceramics Types 5.1. Computer aided design/computer aided machining (CAD/CAM) [CEREC system] 5.2. Copy milling [Celay system]
  • 44. CEREC AC, Sirona Dental System
  • 45. 5.1. CAD/CAM (CEREC system)  In the early 1970s.  Types: 5.1.1. Hard machining 5.1.2. Soft machining  The abutment or die is first scanned.  The computer software designs the restoration.  Then, milling the ceramic block by a computer- aided machine.
  • 46. 5.1.1. Hard machining  For fully sintered ceramic blocks.  Final dimensions of the frameworks can be milled directly.  Advantages * Superior fit (in comparison to soft machining), because no shrinkage is involved in the process. * Produce restorations in one visit.
  • 47. 5.1.2 Soft machining  For partially sintered ceramic blocks, followed by sintering at high temperature.  In 2001.  Enlarged frameworks (about 25%) are milled to compensate for sintering shrinkage.
  • 48. 5.1.2 Soft machining (continued)  Advantages: - Easy to mill. - Save time and tool wear.  Disadvantage: the benefit of fabricating the restoration in one visit is lost, because it requires sintering after machining.  Indications: ceramics difficult to machine such as alumina and zirconia.
  • 49. 5.2. Copy milling [Celay system]  Milled restorations by duplicating a resin pattern using a pantographic device similar to those used for duplicating house keys.  Unable to approach the sophistication of the digital systems (CEREC 3D; Sirona Dental Systems), the Celay system is now obsolete.
  • 50. Types Subtypes Flexural strength (Mpa) Uses 1. Sintered (not available) Alumina-based 140 Replaced by heat pressed or machined all-ceramic restorations Leucite-reinforced 104 2. Castable (not available) 150 Not available 3. Heat- pressed Leucite-reinforced 150 Inlays, onlays, veneers and anterior crowns Lithium disilicate 300 3-unit anterior FPDs, and can extend to the second premolar 4. Glass- infiltrated (slip-cast) In-Ceram Spinel 350–400 Only recommended for anterior crowns In-Ceram Alumina 550 Crowns and 3-unit anterior FPDs In-Ceram Zirconia 650 Posterior crowns and FPDs 5. Machinable (CAD/CAM) 3Y-TZP 900–1200 - Crowns & FPDs. - Orthodontic brackets. - Endodontic posts. - Implants and implant abutments. All-ceramic materials
  • 52.  All-ceramic restorations can be fabricated by both traditional laboratory methods and CAD/CAM.  The traditional laboratory methods * Time consuming. * Technique sensitive. * Unpredictable. * Could not process high strength polycrystalline ceramics such as partially stabilized zirconia.
  • 53. CAD/CAM  Reduce the fabrication time.  A good alternative for both the dentists and laboratories.  Industrially fabricated blocks are more homogenous with minimal flaws.  Can be used for fabrication of both all-ceramic and the veneering porcelain.
  • 54. Types of CAD/CAM ceramics 1. CAD/CAM with feldspathic ceramics 2. CAD/CAM with mica-based ceramics 3. CAD/CAM with leucite-reinforced ceramics 4. CAD/CAM with lithium disilicate reinforced ceramics 5. CAD/CAM with glass-infiltrated alumina and zirconia ceramics
  • 55. 6. CAD/CAM with polycrystalline alumina and zirconia 6.1. Alumina-based polycrystalline ceramics 6.2. Stabilized zirconia-based polycrystalline ceramics 6.2.1. Yttria partially stabilized tetragonal zirconia polycrystals (3Y-TZP) 6.2.2. Magnesia partially stabilized zirconia 6.2.3. Ceria stabilized zirconia/alumina nanocomposite (Ce-TZP/A)
  • 56. 1. CAD/CAM with feldspathic ceramics  Feldspar (Na,K Al Si3O8) as a major crystalline phase: 30 vol%.  Flexural strength: 120 MPa.  Excellent aesthetic properties  Indications: veneers, inlays, onlays and anterior crowns.
  • 57. 1. CAD/CAM with feldspathic ceramics (Continued) 1.1. VitaTM Mark I (Vita Zahnfabrik)  In 1985.  The first CAD/CAM produced inlay & onlay.  Fine grain feldspathic ceramic block.  Fully sintered for hard machining.
  • 58. 1. CAD/CAM with feldspathic ceramics (Continued) 1.2. VitaTM Mark II (Vita Zahnfabrik)  In 1991.  Better mechanical properties.  Flexural strength: 100–160 Mpa.  Made of materials similar to conventional feldspathic ceramic.
  • 59. 2. CAD/CAM with mica-based ceramics  Example: DicorTM MGC.  Mica crystals: 70%.  Flexural strength: about 229 MPa.  Cumulative breakage at 2 years was higher than for VitaTM Mark II.  No longer in the market.
  • 60. 3. CAD/CAM with leucite-reinforced ceramics  Similar in microstructure and mechanical properties to the first generation heat pressed leucite-reinforced ceramics. 3.1. ProCAD (Ivoclar-Vivadent).  In 1998.  Similar in structure, marginal gap and fracture load to the heat-pressed ceramic EmpressTM (Ivoclar-Vivadent).
  • 61. Before and after treatment with all-ceramic restorations (lithium disilicate IPS e.max Press Tooth 24 inlay; onlays 26, 27; and crowns14, 15, 25) and CAD/CAM-fabricated leucite ProCAD onlay 16, 26.
  • 62. 3. CAD/CAM with leucite-reinforced ceramics (continued) 3.2. EmpressTM CAD (Ivoclar-Vivadent)  In 2006.  Leucite crystals: about 45%.  Finer particle size of about 1–5 μm that helps resist machining damages.  The powder is first pressed into blocks and then sintered.
  • 63. 3.2. EmpressTM CAD (continued)  Flexural strength: about 160 MPa.  Indication: chair-side single unit restorations.  Available in: - High Translucency (EmpressTM CAD HT) - Low Translucency (EmpressTM CAD LT) - Polychromatic (EmpressTM CAD Multi)  The milled restoration can be stained and glazed.
  • 64. 4. CAD/CAM with lithium disilicate reinforced ceramics  Example: IPSTM e.max CAD (Ivoclar-Vivadent).  In 2006.  Fully sintered, but partially crystallized.  The block exhibits a flexural strength of 130– 150 MPa in the pre-crystallized (blue) state.  Allows simplified machining and intraoral occlusal adjustment.
  • 65. 4. CAD/CAM with lithium disilicate reinforced ceramics (continued)  Crystallize in a chair-side ceramic oven at 850°C in vacuum for 20–25 min, and changes from blue to the selected shade.  Lithium disilicate crystals: 70 vol%.  Final flexural strength: 300–360 MPa.  Indication: - Chair-side monolithic (full anatomic) anterior and posterior crowns. - Inlay, onlay, and veneer.
  • 66. 5. CAD/CAM with glass-infiltrated ceramics  In 1993.  Presintered blocks to fabricate copings which are further glass-infiltrated. 5.1. CAD/ CAM InCeramTM Spinell  The most translucent of this group .  Flexural strength: 350 MPa.  Indication: anterior crowns.
  • 67. 5.2. CAD/CAM InCeramTM Alumina  Flexural strength: 450–600 MPa.  Marginal gap: 70 μm (clinically acceptable).  Indications: - Anterior and posterior crowns. - 3-unit anterior FPD.
  • 68. 5.3. CAD/CAM InCeramTM Zirconia  Flexural strength: 700 MPa.  Better fit than the slip cast InCeramTM Zirconia.  Indications: the opacity of zirconia has limited its use to the posterior crowns and FPDs.
  • 69. 6. CAD/CAM with polycrystalline alumina and zirconia  Polycrystalline ceramics, such as alumina and zirconia, have no intervening etchable glassy matrix.  The crystals are densely packed, and then sintered.  The dense crystal lattice reduces crack propagation resulting in excellent mechanical properties.  Indications: crown and bridge copings.
  • 70. 6.1. Alumina-based polycrystalline ceramics  Example: ProceraTM AllCeram (Nobel Biocare).  The first fully dense dental polycrystalline ceramic.  In 1993.  More than 99.9% alumina.  Computer-aided production of enlarged die (20%) to compensate for the sintering shrinkage.
  • 71. 6.1. Alumina-based polycrystalline ceramics (continued)  Alumina is densely packed (dry pressed) and then sintered at 1550°C.  Flexural strength: about 600 MPa.  The highest strength of the alumina-based materials, but lower than zirconia.  The highest elastic modulus and hardness of all- ceramic materials.
  • 72. 6.1. Alumina-based polycrystalline ceramics (continued)  Veneered with matched expansion porcelain.  Marginal fit: 70 μm (within the range of clinical acceptance).  Indications: - Veneers. - Crowns. - Anterior FPDs.
  • 73. 6.2. Stabilized zirconia-based polycrystalline ceramics Introduction Advantages of zirconia  High biocompatibility.  High strength and fracture toughness.  Low bacterial surface adhesion  Low thermal conductivity.  Low corrosion potential.  Good radiopacity.
  • 74.  Zirconia is a polymorphic material.  It has three crystallographic forms: * Monoclinic (M): from room temperature to 1170°C. * Tetragonal (T): from 1170°C to 2370°C. * Cubic (C): from 2370°C to the melting point (2715°C).
  • 75.  With the addition of stabilizing oxides such as ceria (CeO2), magnesia (MgO) or yttria (Y2O3), a partially stabilized zirconia (PSZ) is formed at room temperature with cubic crystals as the major phase, and monoclinic and tetragonal crystals as the minor phases.
  • 76.  It is also possible to form a mono-phasic material consisting of tetragonal crystals only, and the material is called tetragonal zirconia polycrystal (TZP).
  • 77. Transformation toughening of zirconia  Stress at the crack tip will trigger transformation from tetragonal to monoclinic phase (T–M transformation).  Accompanied by an increase in volume (about 4.5%) as monoclinic crystals are larger in size.  Induce compressive stress at the crack tip.
  • 78.  Hinder (not totally prevent) the crack propagation.  Resulting in an increase in mechanical properties.  Zirconia has: - High fracture toughness: 9–10 MPa m-1 - High Flexural strength: 900–1200 Mpa (about twice that of alumina).
  • 79. Low temperature degradation (LTD) of zirconia  Progressive spontaneous slow transformation of the metastable tetragonal phase into the monoclinic phase in the presence of water at relatively low temperatures (150–400°C).  Yttria reacts with water vapor to form yttrium hydroxide, resulting in instability of the tetragonal zirconia.
  • 80.  LTD initiates at the surface and subsequently progresses into the bulk of the material.  Accompanied by an increase in volume, which causes stress and microcracking.  Microcracking results in: * Grain pullout. * Surface roughness. * Water penetration. * Decrease in strength (strength degradation).
  • 81.  Factors affecting LTD * Stabilizer type, concentration and distribution. * Grain size. * Residual stresses.  Above a critical grain size, 3Y-TZP is less stable and more susceptible to spontaneous transformation.  Smaller grain sizes are associated with a lower transformation rate.
  • 82.  Higher sintering temperature and time lead to: - Larger grain size. - Higher translucency. - More susceptible to transformation and LTD.
  • 83. Scanning electron micrographs showing the effect of sintering temperature on grain size in 3Y-TZP sintered for 2 hr. (A) 1,300°C; (B) 1,350°C; (C) 1,400°C; (D) 1,450°C; (E) 1,500°C; (F) 1,550°C; (G) 1,600°C; and (H) 1,650°C.
  • 84.  Although some concern was raised by the degradation of femoral heads 20 years ago, no direct correlation has been established between LTD and clinical failure of zirconia in dentistry.
  • 85. 6.2.1. Yttria partially stabilized tetragonal zirconia polycrystals (3Y-TZP)  Yttria: 3 mol%.  Radiopacity is comparable to metal.  Applications - Crowns & FPDs. - Orthodontic brackets. - Endodontic posts. - Implants and implant abutments. - Its use in the esthetic zone is limited to the fabrication of frameworks.
  • 86. 3Y-TZP (continued)  Colored zirconia frameworks are now available, and produce a more clinically acceptable color match.  Examples for partially sintered blanks - LAVATM (3M ESPE). - CerconTM (Dentsply). - e.maxTM ZirCAD (Ivoclar-Vivadent). - ProceraTM Zirconia (NobelBiocare). - VitaTM YZ blocks (Vita Zahnfabrik).
  • 87. 3Y-TZP (continued)  Examples for fully sintered zirconia blocks: DC ZirkonTM (Smartfit Austenal).  Milling the softer partially sintered blanks (green state): - Shortens the milling time. - Reduces the wear of milling tools.  Soft machining of dental restorations requires sintering at 1350–1550°C for 2–6 hours.
  • 88. 3Y-TZP (continued)  Porosity after sintering: less than 0.5 vol%.  Flexural strength: 900–1200 MPa.  Fracture toughness: 9–10 MPa.m0.5  Fully sintered Y-TZP blocks have been processed by hot isostatic pressing. Note: isostatic means equal pressure from every side.
  • 89. 3Y-TZP (continued)  Because of the hardness and poor machinability of fully sintered Y-TZP, a robust milling system and extended milling periods are required.  Milling fully sintered zirconia may compromise the microstructure and strength of the material.
  • 90. 6.2.2. Magnesium partially stabilized zirconia (Mg-PSZ)  Magnesia: 8–10 mol%.  Tetragonal crystals in a cubic matrix.  Decreased stability of the tetragonal phase in a wet environment when compared to 3Y-TZP after veneering.
  • 91. Mg-PSZ (continued)  Lower mechanical properties.  Porosity and large grain size has limited its success.  Example: Denzir-MTM (Dentronic) for hard machining.
  • 92. 6.2.3. Ceria stabilized zirconia/alumina nanocomposite (Ce-TZP/A)  Example: NANOZR.  Alumina: 30 vol%.  Ceria: 10 mol%.  Alumina nanoparticles (10–100 nm) are trapped within zirconia grains, and zirconia nanoparticles (10 nm) are trapped within alumina grains.
  • 93. Microstructure of a conventional Y-TZP (left) and a Ce-TZP/alumina nanocomposite (right).
  • 94. Ce-TZP/A (continued)  Excellent resistance to LTD.  Better mechanical properties than Y-TZP.  Highest flexural strength: about 1400 MPa.  Highest fracture toughness: 19 MPa.m0.5.  Reliable framework for posterior FPDs.
  • 95. Inhibition of crack propagation by stress-induced phase transformation.